# MAH-g-PLA Compatibilization and ATBC Plasticization of Biodegradable PLA/PBAT Blends: A Combined Experimental and Molecular Dynamics Study

“MAH-g-PLA Compatibilization and ATBC Plasticization of Biodegradable PLA/PBAT Blends: A Combined Experimental and Molecular Dynamics Study” (2026), by Hongtao Li et al. Materials Science research paper. Original abstract below, unchanged. A free PDF is available.

- Authors: Hongtao Li, Lishan Kang, Letian Shi, Ni Tang, Mingjun Yang
- Published: November 3, 2026
- Field: Materials Science
- DOI: https://doi.org/10.21203/rs.3.rs-11332121/v1
- Free PDF: https://www.researchsquare.com/article/rs-11332121/latest.pdf

## Abstract

Polylactide/poly(butylene adipate-co-terephthalate) (PLA/PBAT) blends are central to biodegradable packaging. Reactive compatibilization with maleic-anhydride-grafted polylactide (MAH-g-PLA) and plasticization with acetyl tributyl citrate (ATBC) jointly toughen the 70/30 w/w blend; we resolve their combined molecular action by all-atom molecular dynamics on experimentally anchored formulations. Two Flory–Huggins χ routes straddle zero, bracketing a partial-miscibility window consistent with the two amorphous populations resolved by dynamic mechanical analysis (DMA). In the compatibilized blend the succinic-anhydride graft ring localizes on PBAT-rich regions (three-quarters of ring atoms within 0.5 nm of PBAT) while the PLA arm bridges towards PBAT (1.13× enrichment) — a polymeric surfactant consistent with the mechanical optima at 3–5 parts per hundred resin (phr). For the plasticizer, a Fox-quation mass balance of the DMA peak shifts and the simulated 0.5-nm contact statistics independently recover the same ordering: an interfacial/PBAT-associated sink fills first (≈98% of ATBC outside both phase bulks at 1 phr), and direct PLA-phase dissolution grows appreciably only near 5 phr (never exceeding 13% of molecules). At 1–3 phr ATBC anti-plasticizes by occupying free volume without creating it (fractional free volume invariant across loadings and seeds), the structural signature of the experimental ductility minimum. These cross-validated descriptors provide design rules for balancing compatibilizer and plasticizer loadings in foamable PLA blends.

Canonical page: https://nerdi.pages.dev/paper/W7225162515
Read three real papers a day in Nerdi (iPhone): https://apps.apple.com/app/apple-store/id6813826387?pt=128757794&ct=web-paper&mt=8